Customization: | Available |
---|---|
Usage: | Agricultural, Industrial, Household |
Material: | Neoprene |
Still deciding? Get samples of $ !
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Technical index | Neoprene Rubber | Natural Rubber | |
Hardness (IRHD) | 60±5 | 60±5 | |
Strength Tensile (Mpa) | ≥17 | ≥18 | |
Elongation at break (%) | ≥400 | ≥450 | |
Brittleness temperature (ºC) | ≤40 | ≤-50 | |
Constant compression permanent deformation | ≤15 | ≤30 | |
Resistance to ozone aging test (test conditions,20% elongation,40ºC×96h) |
100ppmm | 25ppmm | |
No cracking | No cracking | ||
Hot air aging test (The biggest change comparing with before aging numerical) |
Test conditions (ºC×h) | 100×70 | 70×168 |
Strength Tensile (%) | -15 | -15 | |
Elongation at break(%) | -40 | -20 | |
Variation in hardness(IRHD) | 0,+10 | -5,+10 | |
Strength of rubber and steel Peel adhesive (KN/m) | >10 | >10 | |
Strength of PTFE Slip Sheet and rubber (KN/m) | >7 | >7 |