NO. | ITEM | Result | ||
PN-150 | PN-220 | PN-300 | ||
1 | Expansion rate/%≥ | 150 | 220 | 300 |
2 | Flow at High Temperature (80ºC×5h) | No fiow | No fiow | No fiow |
3 | Low temperature test (-20ºC×5h) | No crack | No crack | No crack |
4 | Peel strength | 0.05MPa | ||
5 | Shear Strength | 1.0MPa | ||
6 | Hydrostatic Pressure | 1.2MPa |
Physical properties | PZ-150 | PZ-250 | PZ-400 | PZ-600 | |
Hardness (shore A) | 42±7 | 42±7 | 45±7 | 48±7 | |
Tensile strength | 3.5 Mpa (min) | 3.5 Mpa (min) | 3 Mpa (min) | 3 Mpa (min) | |
Elongation | 450% (min) | 450% (min) | 350% (min) | 350% (min) | |
Expansion rate | 150% | 250% | 400% | 600% | |
Repeated water immersion test | Tensile strength | 3 Mpa (min) | 3 Mpa (min) | 2 Mpa (min) | 2 Mpa (min) |
Elongation | 350% (min) | 350% (min) | 250% (min) | 250% (min) | |
Expansion rate | 150% | 250% | 300% | 500% | |
Low temperature bending (-20°C*2h) | No crack | No crack | No crack | No crack |